We've detected that you're using an ad content blocking browser plug-in or feature. Ads provide a critical source of revenue to the continued operation of Silicon Investor.  We ask that you disable ad blocking while on Silicon Investor in the best interests of our community.  If you are not using an ad blocker but are still receiving this message, make sure your browser's tracking protection is set to the 'standard' level.
Gold/Mining/Energy : Corner Bay Silver (BAY.T)

 Public ReplyPrvt ReplyMark as Last ReadFilePrevious 10Next 10PreviousNext  
To: Claude Cormier who wrote (919)6/12/2000 1:51:00 PM
From: Elizabeth Andrews  Read Replies (2) of 4409
 
Where was the water from that they used to perform the column tests? Same chemistry as the water at the site?

A heap leach test is 99% more reliable than column leach as there is no compaction and you can't duplicate the weight of a 20 foot heap in the lab. Also what about the clay situation? And did they mention consumption of lime and cyanide?

What's the distribution of silver in the fines?