We've detected that you're using an ad content blocking browser plug-in or feature. Ads provide a critical source of revenue to the continued operation of Silicon Investor.  We ask that you disable ad blocking while on Silicon Investor in the best interests of our community.  If you are not using an ad blocker but are still receiving this message, make sure your browser's tracking protection is set to the 'standard' level.
Pastimes : ceramics-clay-pottery

 Public ReplyPrvt ReplyMark as Last ReadFilePrevious 10Next 10PreviousNext  
To: Peach who wrote (168)2/26/2002 1:30:36 PM
From: AugustWest  Read Replies (2) of 338
 
1650 right now. Starting to put it into a light body reduction for an hour, maybe two if I don't lose temperature with it.

To answer your question. After I hit 2000, it could take up to three hours to reach final temp @2350F. At 2200, I will begin a heavy reduction and turn the gas up full as to not lose temp but rather slowly gain temp until cone 10 melys down. Than I'll back off the heas slightly and let it soak at 2350 for about 20 minutes to allow the glaze to smooth over so I don't end up with a bunch of pin holes on the glaze surfaces.
Report TOU ViolationShare This Post
 Public ReplyPrvt ReplyMark as Last ReadFilePrevious 10Next 10PreviousNext