We've detected that you're using an ad content blocking browser plug-in or feature. Ads provide a critical source of revenue to the continued operation of Silicon Investor.  We ask that you disable ad blocking while on Silicon Investor in the best interests of our community.  If you are not using an ad blocker but are still receiving this message, make sure your browser's tracking protection is set to the 'standard' level.
Gold/Mining/Energy : Precious and Base Metal Investing

 Public ReplyPrvt ReplyMark as Last ReadFilePrevious 10Next 10PreviousNext  
To: russwinter who wrote (6803)1/12/2003 6:11:14 PM
From: loantech  Read Replies (3) of 39344
 
Russ,Bruce, Claude what do you think of this type of mineralization?:
Cu equals copper Zn equals zinc Pb equals lead Ag equals silver
Au equals gold %-percent g/t -grams/tonne ppb - parts per billion
------------------------------------------------------------------------
Length (m) Cu-% Zn-% Pb-% Cu-Zn-Pb-% Ag-g/t Au-ppb
------------------------------------------------------------------------
1 4.96 0.96 1.46 7.38 86 55
------------------------------------------------------------------------
1 0.93 0.50 0.71 2.14 10 38
------------------------------------------------------------------------
1 0.42 1.47 1.44 3.33 8 34
------------------------------------------------------------------------
1 3.07 3.10 0.66 6.83 49 10
------------------------------------------------------------------------
1 4.91 0.40 0.27 5.58 77 27
------------------------------------------------------------------------
1 2.39 0.11 0.08 2.58 31 31
------------------------------------------------------------------------
1 0.80 0.58 0.28 1.66 14 41
------------------------------------------------------------------------
1 0.05 0.95 0.28 1.28 4 31
------------------------------------------------------------------------
1 1.86 1.66 1.34 4.86 27 51
------------------------------------------------------------------------
Average 9 meters 2.15 % 1.08 % 0.72 % 3.95 % 34 g/t 35 ppb
------------------------------------------------------------------------

due diligence grab samples are from a copper-rich portion of the exposed blasted trench at Site 1. Additional grab samples from historical surface showings of VMS mineralization were removed at Site 2 and Site 3 located approximately 400 meters and 500 meters respectively along an apparent north-south strike from Site 1. The ground between the showings is covered by low lying swampy vegetation. significant values are recorded below:

Cu equals copper Zn equals zinc Pb equals lead Co equals cobalt
Ag equals silver Au equals gold %-percent g/t -grams/tonne
ppb - parts per billion
---------------------------------------------------------------------
Location Cu-% Zn-% Pb-% Cu-Zn-Pb -% Co-% Ag-g/t Au -ppb
---------------------------------------------------------------------
Site 1 10.51 0.14 0.38 11.03 0.33 173 15
---------------------------------------------------------------------
Site 1 9.34 0.10 0.26 9.70 0.17 171 11
---------------------------------------------------------------------
Site 1 1.91 0.06 0.51 2.48 0.01 22 20
---------------------------------------------------------------------
Site 1 5.14 0.15 0.09 5.38 0.01 82 16
---------------------------------------------------------------------
Site 1 2.90 0.22 0.22 3.34 0.01 46 14
---------------------------------------------------------------------
Site 1 6.74 0.16 0.08 6.98 0.02 112 12
---------------------------------------------------------------------
Site 1 4.42 0.05 0.13 4.60 0.02 70 10
---------------------------------------------------------------------
Site 1 3.53 0.20 0.15 3.88 0.01 44 16
---------------------------------------------------------------------
Site 1 2.02 0.17 0.85 3.04 0.02 23 98
---------------------------------------------------------------------
Site 2 0.11 6.17 1.28 7.56 0.20 6 9
---------------------------------------------------------------------
Site 2 0.40 5.23 1.11 6.74 0.22 9 7
---------------------------------------------------------------------
Site 2 0.19 3.86 0.79 4.84 0.02 6 11
---------------------------------------------------------------------
Site 3 0.06 2.41 0.01 2.48 0.03 3 1100
---------------------------------------------------------------------
Note: Assays were completed at XRAL Laboratories ( certified to ISO9002
standards ) using conventional assay techniques.