We've detected that you're using an ad content blocking browser plug-in or feature. Ads provide a critical source of revenue to the continued operation of Silicon Investor.  We ask that you disable ad blocking while on Silicon Investor in the best interests of our community.  If you are not using an ad blocker but are still receiving this message, make sure your browser's tracking protection is set to the 'standard' level.
Gold/Mining/Energy : Winspear Resources -- Ignore unavailable to you. Want to Upgrade?


To: Mr Metals who wrote (6023)6/15/1998 9:44:00 AM
From: Philip Nolan  Read Replies (2) | Respond to of 26850
 
238.9 carats recovered from Camsell property

Winspear Resources Ltd WSP
Shares issued 32,726,333 Jun 12 close $0.52
Mon 15 Jun 98 News Release
Mr. John McDonald reports
Winspear Resources advises that 238.9 carats of diamonds have been recovered from processing 199.7 dry tonnes of kimberlite from the NW dyke at Snap Lake, Haywood project, Camsell property.
The Haywood project area is 140 miles northeast of Yellowknife, Northwest Territories. Winspear operates the project on behalf of a joint venture in which Winspear's interest is 57.3 per cent. By completing 1998 budgeted expenditures of $2.68-million, Winspear's interest in the Haywood project will increase to approximately 68 per cent.
During the past winter field season, approximately 100 tonnes of kimberlite from the NW dyke at Snap Lake was obtained from each of two pits that are about 235 metres apart. This material was transported to Yellowknife and processed in the Diavik plant. Results are as follows:

Sample. Dry tonnes Carats
No. processed recovered

64713 (Pit 1) 105.7 90.69
64714 (Pit 2) 94.0 138.21

For both samples, a total of 199.7 dry tonnes were processed for the recovery of 238.9 carats. This yields an average grade of 1.19 carats per dry tonne. A slotted screen measuring 1.0 millimetres by 9.0 millimetres was used as a bottom cut-off size in the processing procedure which is equivalent to a square-mesh cut-off of approximately 1.2 millimetres. The three largest stones recovered weigh 10.87, 8.43, and 6.03 carats, respectively. All are of gem quality. In addition, a further 18 diamonds were recovered that are more than one carat in weight. There is no significant difference in the diamond populations of the two samples.
The main purpose in obtaining this kimberlite sample is to determine whether grade and values are sufficiently promising to proceed with further delineation of the kimberlite dyke. Although results to date are encouraging, initial valuation of the diamonds is required before a decision can be made as to the next step in exploration of this kimberlite dyke.

All diamonds are presently in the process of being valued. These results will be reported when they become available.