We've detected that you're using an ad content blocking browser plug-in or feature. Ads provide a critical source of revenue to the continued operation of Silicon Investor.  We ask that you disable ad blocking while on Silicon Investor in the best interests of our community.  If you are not using an ad blocker but are still receiving this message, make sure your browser's tracking protection is set to the 'standard' level.
Gold/Mining/Energy : Global Platinum & Gold (GPGI) -- Ignore unavailable to you. Want to Upgrade?


To: Scott Wheeler who wrote (6686)7/14/1998 11:36:00 AM
From: go4it  Respond to of 14226
 
Scott,
<<What are some of the potential refinements to the resin column extractions that are/can be initiated? >>

The resin column extraction should be close to 100% efficient. If any refinement were to be done with the process then I would think that it would have to come from the leaching portion of the process.

Chuck



To: Scott Wheeler who wrote (6686)7/14/1998 11:40:00 AM
From: Ron  Read Replies (1) | Respond to of 14226
 
Scott, I can't recall the specific head ore/concentrated ore/ton value calculations. Could you summarize the screening process for me? Recall our visit with Wayne, but I can't find my notes. I understand the actual process after it hits the mill, but its the ore calculation that I am missing. Thanks Ron W